The supercapacitorbased piezoelectric material composite (Na,K)NbO3-CaCu3Ti4O12 (NKN-CCTO) is investigated for possible application in piezoelectric devices. (1-x)NICN-xCCTO (0.015 <= x <= 0.06) with different sintering conditions is researched for supercapacitor based piezoelectric applications. The 0.94NKN-0.06CCTO composite sintered at 975 degrees C shows the highest dielectric permittivity of 796. Clear SEM images of (1-x)NKN-xCCTO reveal that these compositions have high density well-crystallized structures. The composition and sintering temperature dependence of dielectric permittivities and piezoelectric coefficients, plotted in three dimensions, show that the 0.985NKN-0.015CCTO composite sintered at 1025 degrees C has a moderate dielectric permittivity of 405 and a piezoelectric constant of 98 pC/N. (C) 2016 Elsevier Ltd and Techna Group S.r.l. All rights reserved.

키워드

Lead-free piezoelectric; Sintering temperature; Energy harvesting; ELECTRICAL-PROPERTIES; CERAMICS; TEMPERATURE; CUO; MICROSTRUCTURE
제목
(Na,K)NbO3-CaCu3Ti4O12 perovskite composites for supercapacitor based piezoelectric devices
저자
Ji, Jae-Hoon; Lee, Ji-Won; Chung, Hyunsoo; Koh, Jung-Hyuk
DOI
10.1016/j.ceramint.2015.12.010
발행일
2016-03
유형
Article
저널명
Ceramics International
권
42
호
4
페이지
4978 ~ 4983