Enhanced piezoelectric properties of (Bi,Sc)O-3-(Pb,Ti)O-3 ceramics by optimized calcination process

Citations

WEB OF SCIENCE

21
Citations

SCOPUS

19

초록

Enhanced piezoelectric properties of (Bi,Sc)O-3-(Pb,Ti)O-3 (BS-PT) ceramics were prepared under optimized calcination and sintering conditions. Both the calcination and sintering conditions of (Bi,Sc)O-3(Pb,Ti)O-3 ceramics significantly affect the grain size and density, which effects are closely related to the microstructure, piezoelectric, and other properties of the ceramics. The calcination temperature was varied from 720 to 840 degrees C in 30 degrees C increments. Optimizing the calcination temperature improved the piezoelectric coefficient from 388 to 440 pC/N, while improving the relative dielectric constant at 100 Hz from 1401 to 1479. We believe that the optimized calcination process can enhance the piezoelectric properties of (Bi,Sc)O-3-(Pb,(T)i)O-3 ceramics by a very large margin. (C) 2016 Elsevier B.V. All rights reserved.

키워드

Piezoelectric; Calcination; BS-PT; FERROELECTRIC PROPERTIES; PEROVSKITE SYSTEM; TEMPERATURE
제목
Enhanced piezoelectric properties of (Bi,Sc)O-3-(Pb,Ti)O-3 ceramics by optimized calcination process
저자
Ahn, Joong-Hyeon; Koh, Jung-Hyuk
DOI
10.1016/j.jallcom.2016.07.326
발행일
2016-12
유형
Article
저널명
Journal of Alloys and Compounds
권
689
페이지
138 ~ 144