Thermotropic liquid crystal polymer fabric reinforced polyimide composite materials

  • Kim, SH
  • Lim, DK
  • Yi, SC
  • Oh, KW
Citations

WEB OF SCIENCE

2
Citations

SCOPUS

3

초록

An aromatic copolyester thermotropic liquid crystal polymer (LCP) fabric was used to reinforce a polyimide (PI) matrix to produce composites. The LCP/PI composite was made to eliminate directional difference in the mechanical properties of LCP by controlling the individual reinforcement fabric alignment in different directions without losing any mechanical properties. As a result, a transversely isotropic LCP composite material could be obtained from the highly anisotropic LCP fiber. Interfacial adhesion between the LCP and polyimide was greatly improved by a NH3/H-2 plasma treatment on the LCP fabric, thereby the significantly improving mechanical properties of the composite. Moreover, inter-laminar shear strength of the LCP/PI composite was further increased after heat treatment at 220 degreesC for 1 hour. The LCP/polyimide composite retains stable mechanical properties up to 250 degreesC.

제목
Thermotropic liquid crystal polymer fabric reinforced polyimide composite materials
저자
Kim, SHLim, DKYi, SCOh, KW
DOI
10.1002/pc.10235
발행일
2000-10
유형
Article
저널명
Polymer Composites
21
5
페이지
806 ~ 813